Written by the Popper tooling team Notes from our mold shop in Foshan, where we design, machine and test tools for appliance, automotive and medical parts. Last reviewed: 2026-11-20
CAD model of an injection mold showing cooling channels and ejector pins in blue and green
Cooling and ejection layout in a mold design. Wall thickness decides how evenly these channels can work.

Why uniformity matters

Plastic cools by giving up heat through the mold wall. A thick section holds heat longer than a thin one, so it shrinks more and keeps moving after the thin sections have set. That difference shows up as sink marks, voids or warp.

Uniform walls cool at a similar rate, which keeps the part flat and the cycle predictable. When a thicker area is unavoidable, blend into it gradually instead of stepping from thin to thick.

Useful starting ranges

Most common resins work in a band rather than at one exact number. ABS and PC often sit around 2 to 3 mm. PP and PE can run a little thinner. Flow length, part size and the grade of resin shift the right value, so treat these as starting points and confirm with your molder.

Thin walls save material and cool faster but need higher injection pressure and gating. Very thin walls over a long flow can freeze off before the cavity fills.

Common starting wall ranges by resin
ResinTypical wallWatch for
ABS2.0–3.0 mmSink above ribs and bosses
PC2.0–3.0 mmHigh injection pressure
PP1.5–2.5 mmWarp on large flat parts
PE1.5–2.5 mmShrink variation

Ribs instead of solid thickness

Rib rules that hold up

A rib near half the wall thickness works on most parts. Put a small radius where the rib meets the wall. If the rib shows on a cosmetic face, check it under side light on the first sample rather than trusting the CAD file.

If you need stiffness, a thick wall is the wrong tool. Add ribs. A rib around half the thickness of the wall it joins gives most of the stiffness with far less material and a much lower risk of sink.

Thick ribs on a thin wall leave a heavy junction that sinks on the visible face. Keep the rib thin, add a small radius at the base, and the part stays both stiff and clean.

Coring out heavy sections

For a bulky part, remove material from the inside rather than molding a solid block. Coring out shortens cooling time and reduces sink. It also cuts resin cost on every shot, which adds up over a production run.

A mold-flow study can show where the part will cool slowly before steel is cut. It is cheaper to change the CAD file than to rework a tool.

Watch the process

Plastic Injection Molding
Plastic Injection Molding · engineerguy

Questions about your own part? Send us the drawing for a quote.

Read about custom plastic molds →